Mineral: |
Anatase |
Reference: |
LS95a |
SCM Type: |
CC - Constant Capacitance
(C1: 2.66 F/m2) |
Ionic Strength: |
0.1 mol/L of
KNO3
|
Site Type: |
»Ti-OH |
PZC: |
6.58 |
pK1: |
5.4 |
pK1°I=0 (Conversion to I = 0): |
5.29 |
pK12.31 nm−2 (normalized): |
5.02 |
pK2: |
7.75 |
pK2°I=0 (Conversion to I = 0): |
7.64 |
pK22.31 nm−2 (normalized): |
8.13 |
Site Density in nm-2: |
0.9702 |
Original Site Density: |
0.000145 mol / g solid
|
Solid/Liquid Ratio in g/L: |
|
pH Range: |
|
Temperature in K: |
|
Method for Site Density: |
Potentiometric Titration |
Method for Protolysis: | Potentiometric Titration |
Fit Method: | GRFIT |
Comment: |
reactions given as >>S (assumed =>>TiOH); site density confirmed by catechol adsorption; C=2.66+-0.16 F/m^2; also given: pK3 = 17.21 (release of 2 protons from >>S) |
|