Surface Complex Formation Data:

Mineral: Hematite
Reference: EABFY13
SCM Type: DDL - Diffuse Double Layer
Ligand: Eu<3+> - europium(III)
Site Type: »Fe-OH
Equation: 2 »Fe-OH + Eu<3+>  ⇔  (»Fe-O)2-Eu<1+> + 2 H<1+>
LogK: 19.97        LogK°I=0 (Conversion to I = 0):   20.28         LogK2.31 nm−2 (SSD-normalized):   21.84
Experiment: Batch Sorption Experiments
Ionic Strength: 0.01 mol/L NaCl
Temperature: 298.15 K
Solid/Liquid Ratio: 0.5 g/L
pH Range: 3 - 8
Ligand Concentration Range: 3.7E-8 mol/L
Fit Method: FITEQL
Comment: Equilibrium constants referenced to the site-occupancy standard state as suggested by [S03] and calculated using the equation:

K = K((NsAs)²/(NA))*Cs.

Cs is the solid phase concentration in this work (0.5 g/L), Ns and As are the surface site density and surface area measured in this work, 4.28E+18 sites/m² and 30.7 m²/g, respectively. N and A are the hypothetical values suggested by [S03], 10E+18 sites/m² and 10 m²/g, respectively.
 
1 data sets were retrieved