Mineral: |
Magnetite |
Reference: |
JMLGE07 |
SCM Type: |
DDL - Diffuse Double Layer |
Ligand: |
Si(OH)4<0>
- Silicic acid
|
Site Type: |
»Fe-OH |
Equation: |
»Fe-OH + Si(OH)4<0> ⇔ »Fe-H2-SiO4<1-> + H<1+> + H2O |
LogK: |
-3.62 LogK°I=0 (Conversion to I = 0): -3.66
LogK2.31 nm−2 (SSD-normalized): -2.68
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.01 mol/L
NaNO3
|
Temperature: |
298.15 K |
Solid/Liquid Ratio: |
6.0 g/L |
pH Range: |
3.5 - 11 |
Ligand Concentration Range: |
1.12E-4 mol/L |
Fit Method: |
FITEQL |
|