Mineral: |
Goethite |
Reference: |
HHC88 |
SCM Type: |
TL - Triple Layer |
Ligand: |
Th<4+>
- thorium
|
Site Type: |
»Fe-OH |
Equation: |
»Fe-OH + Th<4+> ⇔ »Fe-O-Th<3+> + H<1+> |
LogK: |
1.0 LogK°I=0 (Conversion to I = 0): 3.04
LogK2.31 nm−2 (SSD-normalized): 5.87
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.42 mol/L
NaCl
|
Temperature: |
293.15 K |
Solid/Liquid Ratio: |
0.54 g/L |
pH Range: |
2.5-6.5 |
Ligand Concentration Range: |
9E-6 mol/L |
Fit Method: |
MINEQL |
Comment: |
temperature 20+-2°C; citation in [C96] and [CMFGG98]; experiments also with 4.5E-5M Th |
|