Mineral: |
Kaolinite |
Reference: |
AFI02 |
SCM Type: |
ECC - Extended Constant Capacitance |
Ligand: |
phthal<2->
- o-phthalate
|
Site Type: |
»X-OH |
Equation: |
»X-OH + phthal<2-> + 2 H<1+> ⇔ »X-OH2-phthal-H |
LogK: |
11.3 LogK°I=0 (Conversion to I = 0): 11.50
LogK2.31 nm−2 (SSD-normalized): 10.89
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.005 mol/L
KNO3
|
Temperature: |
298.15 K |
Solid/Liquid Ratio: |
2.02 g/L |
Fit Method: |
FITEQL |
Comment: |
outer sphere complex;temperature 25+-0.5°C; solid concentration 100 m^2/L (49.6m^2/g); FITEQL/GRFIT |
|