RES³T - Rossendorf Expert System for Surface and Sorption Thermodynamics

Show Detailed Complexation Query Results


Surface Complex Formation Data:

Mineral: Montmorillonite
Reference: G02a
SCM Type: CC - Constant Capacitance
Ligand: AsO3<3-> - arsenite
Site Type: »X-OH
Equation: »X-OH + AsO3<3-> + 3 H<1+>  ⇔  »X-H2AsO3 + H2O
LogK: 35.89        LogK°I=0 (Conversion to I = 0):   36.43         LogK2.31 nm−2 (SSD-normalized):   35.70
Experiment: Batch Sorption Experiments
Ionic Strength: 0.01 mol/L NaCl
Fit Method: FITEQL
Comment: original reaction equation in the study: »X-OH + H3AsO3 = »X-H2AsO3 + H2O with logK = 1.19, formation constant in aqueous solution: H3AsO3 = AsO3<3-> + 3H<1+> with logK = -34.7 [MBK00]
 
1 data sets were retrieved