Surface Complex Formation Data:

Mineral: Hematite
Reference: SVYT03
SCM Type: TL - Triple Layer
Ligand: Na<1+> - sodium
Site Type: »Fe-OH
Equation: »Fe-OH + Na<1+>  ⇔  »Fe-O-Na + H<1+>
LogK: -1.01        LogK°I=0 (Conversion to I = 0):   -1.01         LogK2.31 nm−2 (SSD-normalized):   -0.07
Experiment: Batch Sorption Experiments
Ionic Strength: 0.001 mol/L NaNO3
Temperature: 298.0 K
Solid/Liquid Ratio: 10.0 g/L
Ligand Concentration Range: 0.001 mol/L
Fit Method: KINEQL
Comment: mineral unspecified: ferric oxide; temperature 25+-1°C
 