Mineral: |
Hematite |
Reference: |
SVYT03 |
SCM Type: |
TL - Triple Layer |
Ligand: |
Cu<2+>
- copper
|
Site Type: |
»Fe-OH |
Equation: |
»Fe-OH + Cu<2+> + H2O ⇔ »Fe-O-Cu(OH) + 2 H<1+> |
LogK: |
-2.5 LogK°I=0 (Conversion to I = 0): -2.47
LogK2.31 nm−2 (SSD-normalized): -1.56
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.001 mol/L
NaNO3
|
Temperature: |
298.0 K |
Solid/Liquid Ratio: |
10.0 g/L |
pH Range: |
2-10 |
Ligand Concentration Range: |
6.4E-5 mol/L |
Fit Method: |
KINEQL |
Comment: |
also data for surface polymer model and continuum model; mineral unspecified: ferric oxide; temperature 25+-1°C |
|