Mineral: |
Goethite |
Reference: |
MG96b |
SCM Type: |
CC - Constant Capacitance |
Ligand: |
MoO4<2->
- molybdate
|
Site Type: |
»Fe-OH |
Equation: |
»Fe-OH + H2MoO4 ⇔ »Fe-HMoO4 + H2O |
LogK: |
7.9 LogK°I=0 (Conversion to I = 0): 8.54
LogK2.31 nm−2 (SSD-normalized): 12.58
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.1 mol/L
NaCl
|
Temperature: |
296.15 K |
Solid/Liquid Ratio: |
2.5 g/L |
pH Range: |
2.5-11 |
Ligand Concentration Range: |
2.66E-4 mol/L |
Fit Method: |
FITEQL |
Comment: |
one-site approach (monodentate only) |
|