Surface Complex Formation Data:

Mineral: Gibbsite
Reference: MG96b
SCM Type: CC - Constant Capacitance
Ligand: AsO4<3-> - arsenate
Site Type: »Fe-OH
Equation: »Fe-OH + AsO4<3-> + 3 H<1+>  ⇔  »Al-H2AsO4 + H2O
LogK: 14.92        LogK°I=0 (Conversion to I = 0):   16.20
Experiment: Batch Sorption Experiments
Ionic Strength: 0.1 mol/L NaCl
Temperature: 296.15 K
Solid/Liquid Ratio: 2.5 g/L
pH Range: 2.5-11
Ligand Concentration Range: 2.66E-4 mol/L
Fit Method: FITEQL
Comment: two-site approach (monodentate and bidentate); original reaction equation in the study: »Al-OH + H3AsO4 = »Al-H2AsO4 + H2O with logK = -5.7, formation constant in aqueous solution: AsO4<3-> + 3 H<+> = H3AsO4<0> logK = 20.62 [GFFGN03]
 