RES³T - Rossendorf Expert System for Surface and Sorption Thermodynamics

Show Detailed Complexation Query Results


Surface Complex Formation Data:

Mineral: Alumina
Reference: NS06
SCM Type: DDL - Diffuse Double Layer
Ligand: Fe<2+> - iron(II)
Site Type: »Al(s)-OH
Equation: »Al(s)-OH + Fe<2+>  ⇔  »Al(s)-O-Fe<1+> + H<1+>
LogK: -0.66 ± 0.03         LogK°I=0 (Conversion to I = 0):   -0.66         LogK2.31 nm−2 (SSD-normalized):   -4.89
Experiment: Batch Sorption Experiments
Ionic Strength: 0.0 mol/L
Temperature: 298.15 K
pH Range: 4-9
Ligand Concentration Range: 0.2-5E-4 mol/L
Fit Method: FITEQL
Comment: mineral loading 0-10 g/L; uncertainty: one standard deviation; experimental ionic strength 0.001-0.1M
 
1 data sets were retrieved