Mineral: |
Goethite |
Reference: |
PVEKF08 |
SCM Type: |
CC - Constant Capacitance |
Ligand: |
Cu<2+>
- copper
|
Site Type: |
»Fe-OH |
Equation: |
»Fe-OH + Cu<2+> ⇔ »Fe-O-Cu<1+> + H<1+> |
LogK: |
2.2 ± 0.2
LogK°I=0 (Conversion to I = 0): 2.33
LogK2.31 nm−2 (SSD-normalized): 2.92
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.01 mol/L
NaNO3
|
Temperature: |
298.15 K |
Solid/Liquid Ratio: |
33.0 g/L |
pH Range: |
2-10 |
Ligand Concentration Range: |
8.2E-6 mol/L |
Fit Method: |
MINTEQA2 |
Comment: |
76.6 m2/L goethite surface |
|