Mineral: |
Alumina |
Reference: |
ZB04b |
SCM Type: |
NE - Non-electrostatic |
Ligand: |
Pu<4+>
- plutonium(IV)
|
Site Type: |
»Al-OH |
Equation: |
»Al-OH + Pu<4+> + H2O ⇔ »Al-O-PuO<1+> + 3 H<1+> |
LogK: |
5.95 ± 0.47
LogK2.31 nm−2 (SSD-normalized): 4.56
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
|
Temperature: |
298.15 K |
Ligand Concentration Range: |
6E-10. 2E-10. 6E-08 mol/L |
Fit Method: |
FITEQL |
Comment: |
average non-electrostatic SC constant for aluminosilicates of 4 curves from [RBAB91], [AOTKA82] and [S83c]; standard deviation relate to the differences in fitted logK constants from the various batch sorption data sets; IS was 0.01 and 0.1 M; surface complexation to aluminosilicate >SiOH or >AlOH reactive sites is considered equivalent to the reactivity of aluminum oxide and silica reactive sites. |
|