Mineral: |
Magnetite |
Reference: |
GM06 |
SCM Type: |
DDL - Diffuse Double Layer |
Ligand: |
Cs<1+>
- cesium
|
Site Type: |
»Fe-OH |
Equation: |
»Fe-OH + Cs<1+> ⇔ »Fe-OH-Cs<1+> |
LogK: |
1.05
LogK2.31 nm−2 (SSD-normalized): 1.99
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
NaClO4
|
Temperature: |
298.15 K |
Fit Method: |
CHESS |
Comment: |
sorption edges (pH 3 to 13.5; IS was 0.001, 0.01, 0.1; Cs conc. = 3E-09 M; S/L ratio was 2 and 10 g/L) and sorption isotherms (fixed pH of 9.4; Cs conc. From 1E-10 to 1E-06 M; IS = 1E-03 M) were measured; SSA, SSD and protolysis constants from [MGF03] |
|