Mineral: |
Alumina |
Reference: |
GYXW09 |
SCM Type: |
DDL - Diffuse Double Layer |
Ligand: |
UO2<2+>
- uranyl(VI)
|
Site Type: |
»Al-OH |
Equation: |
»Al-OH + UO2<2+> ⇔ »Al-O-UO2<1+> + H<1+> |
LogK: |
1.4
LogK2.31 nm−2 (SSD-normalized): 0.01
|
Ionic Strength: |
|
Temperature: |
295.15 K |
pH Range: |
2.2 - 9.5 |
Ligand Concentration Range: |
1.04E-4; 2.61E-5; 7.5E-5 mol/L |
Fit Method: |
PHREEQC |
Comment: |
S/L ratio 2 and 10 g/L; IS was 0.01, 0.05, 0.1 and 0.5 mol/L NaCl or 0.1 mol/L NaNO3; sorption edges and sorption isotherms |
|