Mineral: |
Bentonite |
Reference: |
GXSTW09 |
SCM Type: |
DDL - Diffuse Double Layer |
Ligand: |
Eu<3+>
- europium(III)
|
Site Type: |
»Al(w)-OH |
Equation: |
»Al(w)-OH + Eu<3+> ⇔ »Al(w)-O-Eu<2+> + H<1+> |
LogK: |
-2.0
LogK2.31 nm−2 (SSD-normalized): -1.88
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
NaCl
|
Temperature: |
298.15 K |
pH Range: |
2-11 |
Ligand Concentration Range: |
6.74E-8 and 3.33E-6 mol/L |
Fit Method: |
FITEQL |
Comment: |
Na-bentonite; IS: 0.01, 0.1 and 0.5 mol/L of NaCl; S/L ratio: 0.25, 0.5, 1.0 g/L |
|