RES³T - Rossendorf Expert System for Surface and Sorption Thermodynamics

Show Detailed Complexation Query Results


Surface Complex Formation Data:

Mineral: Hematite
Reference: RK14
SCM Type: DDL - Diffuse Double Layer
Ligand: Cu<2+> - copper
Site Type: »Fe-OH
Equation: »Fe-OH + Cu<2+>  ⇔  »Fe-O-Cu<1+> + H<1+>
LogK: -0.65        LogK°I=0 (Conversion to I = 0):   -0.33         LogK2.31 nm−2 (SSD-normalized):   0.29
Experiment: Batch Sorption Experiments
Ionic Strength: 0.1 mol/L NaNO3
Temperature: 298.15 K
Solid/Liquid Ratio: 3.33 g/L
pH Range: 2-7
Fit Method: FITEQL
Comment: recalculated values from [PS04c], with input parameters reported in the original papers, 25 ppm [Cu]total
 
1 data sets were retrieved