Mineral: |
Hydrotalcite |
Reference: |
WAT01c |
SCM Type: |
DDL - Diffuse Double Layer |
Ligand: |
TcO4<1->
- technate
|
Site Type: |
»X-OH |
Equation: |
»X-OH + TcO4<1-> + H<1+> ⇔ »X-OH2-TcO4 |
LogK: |
15.33 ± 0.23
LogK°I=0 (Conversion to I = 0): 15.42
LogK2.31 nm−2 (SSD-normalized): 15.14
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.01 mol/L
|
Temperature: |
298.15 K |
Solid/Liquid Ratio: |
0.59 g/L |
pH Range: |
10-13 |
Ligand Concentration Range: |
1.4E-5 mol/L |
Fit Method: |
FITEQL |
Comment: |
Hydrotalcit-like material Mg6Al2O9; experimental data from [KRMNF96] |
|