Mineral: |
Alumina |
Reference: |
KRKTM11 |
SCM Type: |
CC - Constant Capacitance |
Ligand: |
TcO<2+>
- technetium(IV)
|
Site Type: |
»Al-OH |
Equation: |
»Al-OH + TcO<2+> + H2O ⇔ »Al-O-TcO(OH) + 2 H<1+> |
LogK: |
-1.01 LogK°I=0 (Conversion to I = 0): -0.80
LogK2.31 nm−2 (SSD-normalized): 0.20
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.1 mol/L
NaClO4
|
Solid/Liquid Ratio: |
5.0 g/L |
pH Range: |
3-10 |
Ligand Concentration Range: |
1E-12 mol/L |
Fit Method: |
FITEQL |
Comment: |
wrong equation in the article: »Al-OH + TcO<2+> + H2O = »Al-O-TcO(OH); reducing conditions simulated with [Sn(II)] = 1E-6 M |
|