Show Detailed Complexation Query Results
Surface Complex Formation Data:
Mineral: |
Alumina |
Reference: |
H17 |
SCM Type: |
NE - Non-electrostatic |
Ligand: |
SeO3<2->
- selenite
|
Site Type: |
»Al(w)-OH |
Equation: |
»Al(w)-OH + SeO3<2-> + Na<1+> ⇔ »Al(w)-O-Na-SeO3<2-> + H<1+> |
LogK: |
-5.2 LogK°I=0 (Conversion to I = 0): -5.20
LogK2.31 nm−2 (SSD-normalized): -5.08
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.0 mol/L
NaClO4
|
Temperature: |
294.15 K |
Solid/Liquid Ratio: |
0.5 g/L |
pH Range: |
3-11 |
Ligand Concentration Range: |
1E-10 - 1E-3 mol/L |
Fit Method: |
CHESS |
Comment: |
Ionic strength: Edge: 5·10-4 - 5·10-1 M NaClO4, NaCl, NaHCO3, NaNO3 and Na2SO4
Isotherm:: 1·10-1 M NaClO4 |
|
1 data sets were retrieved
|