Show Detailed Complexation Query Results
Surface Complex Formation Data:
Mineral: |
Alumina |
Reference: |
H17 |
SCM Type: |
NE - Non-electrostatic |
Ligand: |
UO2<2+>
- uranyl(VI)
|
Site Type: |
»Al(w)-OH |
Equation: |
»Al(w)-OH + UO2<2+> + H2O ⇔ »Al(w)-O-UO2(OH) + 2 H<1+> |
LogK: |
-4.2 LogK°I=0 (Conversion to I = 0): -4.20
LogK2.31 nm−2 (SSD-normalized): -4.08
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.0 mol/L
NaClO4
|
Temperature: |
294.15 K |
Solid/Liquid Ratio: |
1.0 g/L |
pH Range: |
3-11 |
Ligand Concentration Range: |
4E-7 mol/L |
Fit Method: |
CHESS |
|
1 data sets were retrieved
|