Mineral: |
Alumina |
Reference: |
H17 |
SCM Type: |
NE - Non-electrostatic |
Ligand: |
UO2<2+>
- uranyl(VI)
|
Site Type: |
»Al(w)-OH |
Equation: |
»Al(w)-OH + UO2<2+> + Na<+> + 2 CO3<2-> ⇔ »Al(w)-O-Na-UO2(CO3)2<2-> + H<1+> |
LogK: |
16.6576 LogK°I=0 (Conversion to I = 0): 16.66
LogK2.31 nm−2 (SSD-normalized): 16.77
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.0 mol/L
NaClO4
|
Temperature: |
294.15 K |
Solid/Liquid Ratio: |
1.0 g/L |
pH Range: |
3-11 |
Ligand Concentration Range: |
4E-7 mol/L |
Fit Method: |
CHESS |
Comment: |
Original equation:
>SWOH − 3H+ + UO22+ + 2HCO3− + Na+ ⇌ SWO−Na−UO2(CO3)22−
logK° = -4 |
|