Mineral: |
Magnetite |
Reference: |
LSLCH17 |
SCM Type: |
DDL - Diffuse Double Layer |
Ligand: |
UO2<2+>
- uranyl(VI)
|
Site Type: |
»Fe-OH |
Equation: |
2 »Fe-OH + UO2<2+> + 2 H2O ⇔ (»Fe-O)2-UO2(OH)2<2-> + 4 H<1+> |
LogK: |
-3.97 LogK°I=0 (Conversion to I = 0): -3.97
LogK2.31 nm−2 (SSD-normalized): -2.10
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.01 mol/L
NaCl
|
Temperature: |
298.15 K |
Solid/Liquid Ratio: |
1.0 g/L |
pH Range: |
2-11 |
Ligand Concentration Range: |
3.703E-5 mol/L |
Fit Method: |
FITEQL |
Comment: |
c(UO22+) = 10 mg/L |
|