Surface Complex Formation Data:

Mineral: Hematite
Reference: CMFGG98
SCM Type: DDL - Diffuse Double Layer
Ligand: Th<4+> - thorium
Site Type: »Fe-OH
Equation: »Fe-OH + Th<4+>  ⇔  »Fe-OH-Th<4+>
LogK: 18.7 ± 1.2         LogK°I=0 (Conversion to I = 0):   18.70         LogK2.31 nm−2 (SSD-normalized):   24.14
Experiment: Batch Sorption Experiments
Ionic Strength: 0.0 mol/L NaClO4
pH Range: 2-10
Fit Method: FITEQL
Comment: I = 0.01 and 0.1 M; constant is calculated by applying the SIT for I = 0; mean value; set of hydrolysis constants for Th from [BM76]; carbonate concentration 5E-5M; other logK (apparent/intrinsic): 18.8/19.5 (0.01M), 16.0/17.8 (0.1M)
 
1 data sets were retrieved