Mineral: |
Calcite |
Reference: |
PPS04 |
SCM Type: |
CC - Constant Capacitance |
Ligand: |
Ga<3+>
- gallium
|
Site Type: |
»Ca-OH |
Equation: |
»Ca-OH + Ga<3+> + 5 H2O ⇔ »Ca-H9GaO6<1+> + 2 H<1+> |
LogK: |
7.0 LogK°I=0 (Conversion to I = 0): 7.00
LogK2.31 nm−2 (SSD-normalized): 2.25
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.0 mol/L
|
Temperature: |
298.15 K |
pH Range: |
6 - 12 |
Ligand Concentration Range: |
1E-4 - 5E-4; 12E-6 - 24E-6; 14E-9 mol/L |
Fit Method: |
MINTEQA2 |
Comment: |
logK = 7.0 ± 0.3-3.19; 25 g/L, 6.7 g/L, 100 g/L |
|