| Mineral: |
Baddeleyite (Zirconia) |
| Reference: |
LDS03 |
| SCM Type: |
CC - Constant Capacitance |
| Ligand: |
UO2<2+>
- uranyl(VI)
|
| Site Type: |
»Zr-OH |
| Equation: |
3 »Zr-OH + UO2NO3<1+> ⇔ (»Zr-OH)3-UO2NO3<1+> |
| LogK: |
10.0 LogK°I=0 (Conversion to I = 0): 10.67
LogK2.31 nm−2 (SSD-normalized): 11.91
|
| Experiment: |
Batch Sorption Experiments |
| Ionic Strength: |
0.5 mol/L
|
| Temperature: |
298.15 K |
| Solid/Liquid Ratio: |
20.0 g/L |
| pH Range: |
1-6 |
| Ligand Concentration Range: |
1.1E-5 mol/L |
| Fit Method: |
FITEQL |
| Comment: |
background electrolyte NaClO4 or KNO3 (difference, presence of uranyl nitrate complex sorbed on baddeleyite) |
| |