| Mineral: |
Montmorillonite |
| Reference: |
TNOYS10 |
| SCM Type: |
DDL - Diffuse Double Layer |
| Ligand: |
NpO2<1+>
- neptunyl(V)
|
| Site Type: |
»X-OH |
| Equation: |
»X-OH + NpO2<1+> + CO3<2-> ⇔ »X-O-NpO2CO3<2-> + H<1+> |
| LogK: |
1.33 LogK°I=0 (Conversion to I = 0): 1.76
LogK2.31 nm−2 (SSD-normalized): 5.22
|
| Experiment: |
Batch Sorption Experiments |
| Ionic Strength: |
0.1 mol/L
NaNO3
|
| Temperature: |
298.15 K |
| Solid/Liquid Ratio: |
4.0 g/L |
| Ligand Concentration Range: |
9.25E-07 mol/L |
| Fit Method: |
FITEQL |
| Comment: |
based on data from TPB98 |
| |