| Mineral: |
Alumina |
| Reference: |
MMHM12 |
| SCM Type: |
DDL - Diffuse Double Layer |
| Ligand: |
Eu<3+>
- europium(III)
|
| Site Type: |
»Al-OH |
| Equation: |
»Al-OH + Eu<3+> ⇔ »Al-O-Eu<2+> + H<1+> |
| LogK: |
-1.2 LogK°I=0 (Conversion to I = 0): -0.34
LogK2.31 nm−2 (SSD-normalized): -2.59
|
| Experiment: |
Batch Sorption Experiments |
| Ionic Strength: |
0.1 mol/L
NaNO3
|
| Temperature: |
298.15 K |
| Solid/Liquid Ratio: |
4.0 g/L |
| Ligand Concentration Range: |
1E-03 mol/L |
| Fit Method: |
FITEQL |
| Comment: |
at 25°C; protolysis data modeled by using the contant capacitance model [MDCF94] |
| |