| Mineral: |
Goethite |
| Reference: |
ZB04a |
| SCM Type: |
NE - Non-electrostatic |
| Ligand: |
PuO2<1+>
- plutonyl(V)
|
| Site Type: |
»Fe-OH |
| Equation: |
»Fe-OH + PuO2<1+> + H2O ⇔ »Fe-OH-PuO3<1-> + 2 H<1+> |
| LogK: |
-10.66 LogK°I=0 (Conversion to I = 0): -10.77
LogK2.31 nm−2 (SSD-normalized): -9.72
|
| Experiment: |
Batch Sorption Experiments |
| Ionic Strength: |
0.1 mol/L
NaNO3
|
| Temperature: |
293.15 K |
| Ligand Concentration Range: |
1E-11. 1E-10 mol/L |
| Fit Method: |
FITEQL |
| Comment: |
average non-electrostatic SC constant of 2 curves from [SMS85]; standard deviation could not be calculated with less than 3 data sets |
| |