| Mineral: |
Quartz |
| Reference: |
PTBP98 |
| SCM Type: |
DDL - Diffuse Double Layer |
| Ligand: |
UO2<2+>
- uranyl(VI)
|
| Site Type: |
»Si-OH |
| Equation: |
»Si-OH + 3 UO2<2+> + 5 H2O ⇔ »Si-O-(UO2)3(OH)5 + 6 H<1+> |
| LogK: |
-16.75 LogK°I=0 (Conversion to I = 0): -16.11
|
| Experiment: |
Batch Sorption Experiments |
| Ionic Strength: |
0.1 mol/L
NaNO3
|
| Temperature: |
293.15 K |
| pH Range: |
2-9 |
| Ligand Concentration Range: |
2E-7 - 2E-6 mol/L |
| Fit Method: |
FITEQL |
| Comment: |