| Mineral: |
Kaolinite |
| Reference: |
LKLSD09 |
| SCM Type: |
DDL - Diffuse Double Layer |
| Ligand: |
Co<2+>
- cobalt(II)
|
| Site Type: |
»X-OH |
| Equation: |
»X-OH + Co<2+> ⇔ »X-O-Co<1+> + H<1+> |
| LogK: |
-3.9
LogK2.31 nm−2 (SSD-normalized): -4.09
|
| Experiment: |
Batch Sorption Experiments |
| Ionic Strength: |
NaNO3
|
| Temperature: |
298.0 K |
| Solid/Liquid Ratio: |
5.0 g/L |
| pH Range: |
2-10 |
| Ligand Concentration Range: |
1E-4 - 1E-6 mol/L |
| Fit Method: |
FITEQL |
| Comment: |
KGa-1b Kaolinite, monodentate variable charge site |
| |