Show Detailed Complexation Query Results
Surface Complex Formation Data:
| Mineral: |
Alumina |
| Reference: |
HS73 |
| SCM Type: |
DDL - Diffuse Double Layer |
| Ligand: |
Sr<2+>
- strontium
|
| Site Type: |
»Al-OH |
| Equation: |
»Al-OH + Sr<2+> ⇔ »Al-O-Sr<1+> + H<1+> |
| LogK: |
-6.27 LogK°I=0 (Conversion to I = 0): -5.95
LogK2.31 nm−2 (SSD-normalized): -3.94
|
| Experiment: |
Potentiometric Titration |
| Ionic Strength: |
0.1 mol/L
NaCl
|
| Temperature: |
298.15 K |
| Fit Method: |
| Comment: |
also electrophoretic measurements and sorption isotherms performed; temperature 25+-2°C, SCM type not clear, SCM type not clear (maybe also NEM) |
| |
1 data sets were retrieved
|