SANS investigations of the irradiation-caused structural damages in VVER 440-type reactor pressure vessel steels


SANS investigations of the irradiation-caused structural damages in VVER 440-type reactor pressure vessel steels

Böhmert, J.; Große, M.; Nitzsche, P.

Small-angle neutron scattering (SANS) experiments were performed at KWS2 facility of the KFA Jülich for investigating the defect structures, which are produced by neutron irradiation in Russian Cr-Mo-V alloyed reactor pressure vessel steel. Irradiation and post-irradiation annealing considerably change both SANS intensity and its course in the Guinier plot, which was analysed by the Glatter method. As a rule, bimodal size distribution functions were found with a first maximum at a radius of 1-2 nm and a second maximum at 6-8 nm. Irradiation increases the first maximum, annealing reduced it.

  • Physica B 234 - 236 (1997), 997 - 998