Mineral: |
Montmorillonite |
Reference: |
GSF98 |
SCM Type: |
CC - Constant Capacitance |
Ligand: |
MoO4<2->
- molybdate
|
Site Type: |
»Al-OH |
Equation: |
»Al-OH + H2MoO4 ⇔ »Al-HMoO4 + H2O |
LogK: |
8.43 LogK°I=0 (Conversion to I = 0): 8.86
LogK2.31 nm−2 (SSD-normalized):
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.1 mol/L
NaCl
|
Temperature: |
296.15 K |
Fit Method: |
FITEQL |
Comment: |
23+-1°C; raw data [GFG96], data of [GFG96] are reanalyzed using Mo(ads) as \"dummy\" component; improved fit |
|