RES³T - Rossendorf Expert System for Surface and Sorption Thermodynamics

Show Detailed Site Query Results


Binding Site Data:


Mineral: Hematite
Reference: KAKVC18
SCM Type: CDM - (CD-)MUSIC   (C1: 1.86 F/m2,  C2: 2.0 F/m2)
Ionic Strength: NaNO3
Site Type: »Fe-singly
PZC: 7.32
pK1: 7.32   pK12.31 nm−2 (normalized): 7.09
pK2:   
Site Density in nm-2: 1.3489
Original Site Density: 2.24 µmol / m² surface
Solid/Liquid Ratio in g/L: 0.2
pH Range: 3-8
Temperature in K: 298.0
Method for Site Density: Manual Modification
Method for Protolysis:Assumption
Fit Method:ECOSAT
Comment: ionic strengths 0.001, 0.01, 0.1 M NaNO3; SSD refined to obtain slightly higher values for all the Fe oxides, for optimization of SSD all proton and metal binding data sets were used; both reactive groups, >FeOH<0.5-> and >Fe3OH<0.5->, have the same reactivity with protons, no differentiation was assumed between crystal faces, >Fe2OH sites are non-reactive; logK(H) = PZC
 
1 data sets were retrieved