Mineral: |
Goethite |
Reference: |
DLLSM18 |
SCM Type: |
CDM - (CD-)MUSIC |
Ligand: |
PO4<3->
- phosphate
|
Site Type: |
»Fe-singly |
Equation: |
»Fe-OH<0.5-> + PO4<3-> + 2 H<1+> ⇔ »Fe-O-PO2OH<1.5-> + H2O |
LogK: |
27.34 LogK°I=0 (Conversion to I = 0): 28.52
LogK2.31 nm−2 (SSD-normalized):
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.1 mol/L
NaCl
|
Temperature: |
298.15 K |
Solid/Liquid Ratio: |
1.1 g/L |
pH Range: |
3 - 12 |
Ligand Concentration Range: |
1.4E-4; 2E-4; 3.9E-4 mol/L |
Fit Method: |
ECOSAT + FIT |
Comment: |
z1 = 0.46, z2 = -1.46, z2 = 0 [SHV06b] |
|