Mineral: |
amorphous Al(OH)₃ |
Reference: |
K97d |
SCM Type: |
DDL - Diffuse Double Layer |
Ligand: |
Cu<2+>
- copper
|
Site Type: |
»Al(w)-OH |
Equation: |
2 »Al(w)-OH + Cu<2+> ⇔ (»Al(w)-O)2-Cu + 2 H<1+> |
LogK: |
-3.65
LogK2.31 nm−2 (SSD-normalized): 0.15
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
|
Temperature: |
291.15 K |
pH Range: |
5-6.5 |
Fit Method: |
Comment: |
formation of bi-dentate complex; model starts to diverge from data at removal levels above 40% (pH 6.5), temperature 18+-0.5°C |
|