Mineral: |
Hematite |
Reference: |
RK14 |
SCM Type: |
DDL - Diffuse Double Layer |
Ligand: |
La<3+>
- lanthanum
|
Site Type: |
»Fe-OH |
Equation: |
»Fe-OH + La<3+> ⇔ »Fe-O-La<2+> + H<1+> |
LogK: |
-0.65 LogK°I=0 (Conversion to I = 0): 0.21
LogK2.31 nm−2 (SSD-normalized): 0.29
|
Experiment: |
Batch Sorption Experiments |
Ionic Strength: |
0.1 mol/L
NaNO3
|
Ligand Concentration Range: |
2E-5 mol/L |
Fit Method: |
FITEQL |
Comment: |
recalculated values from [MF99], with input parameters reported in the original papers |
|